6 Star Metal Ingot Bar - Lead free Low Melting Point Tin Bismuth alloy

(1 review) Write a Review

Bulk discount rates

Below are the available bulk discount rates for each individual item when you purchase a certain amount

Buy 3 - 9 and pay only €6.43 each
Buy 10 - 29 and pay only €5.02 each
Buy 30 - 99 and pay only €4.51 each
Buy 100 or above and pay only €4.05 each

Options

€8.50
Inc. Sales Tax
€6.91
Ex. Sales Tax
Or

Info

SKU:PA2083 ,UPC: ,Weight: ,Shipping:

Info

SKU:
PA2083
UPC:
0735930020834
MPN:
PA2083
Weight:
0.11 KGS
Shipping:
Calculated at Checkout

Specifications

Commodity Manufacturer Country, Commodity Code, Commodity Description,

Specifications

Commodity Manufacturer Country:
IRL
Commodity Code:
82060000
Commodity Description:
Hobby Casting Metal

Description

6-Star Metal is a low melting point alloy for home-casting of miniatures. It contains 40% Tin SN and 60% Bismuth BI and is non toxic.  Castings are safe to handle for children but beware of that small children can swallow small pieces.  The metal is hard and miniatures cannot be bended.

Lowest melting point of any home casting metal.  Can be molten on a domestic cooker

Allow 2-3 minutes before releasing from a mould.

Ingot length 122 mm, Width 25mm, weight 100gr approximately (bar weight may vary slightly by a few gram.)

Melts at 140°C (284°F).

Cast at 300-370°C. (572F-698F)

Melts on electric cooker at maximum. For very fine detailed casting we recommend our Solder Melting Pot which can bring up temperature up higher. 

  • 25-28mm scale = 10 single unmounted figures
  • 40mm scale = 5 single unmounted figures
  • 54mm scale = 3 single unmounted figures

All our casting metal come in same size bars. So above chart is valid for Standard, 5Star, 6Star and Model Metal.

Safety Precautions:

  • Adult supervision recommended for children under the age of 16.
  • Hot metal will burn if touched or spilled.
  • Cover the working surface with paper or hard board.
  • Do not leave a ladle with molten metal unattended
  • Do not overheat the metal with a gas flame.
  • Never cool the metal or moulds with water.

Frequently Bought Together:

6 Star Tin Bismuth Alloy ingot
Inc. Sales Tax
Ex. Sales Tax

1 Review

View All
  • 4
    6 STAR METAL INGOT BAR - LEAD FREE LOW MELTING POINT TIN BISMUTH ALLOY

    Great

1 Review

  • 4
    6 STAR METAL INGOT BAR - LEAD FREE LOW MELTING POINT TIN BISMUTH ALLOY

    Great

Videos