Description | Standard metal (65% Lead / 2% Antimony / 33% Tin) is the cheapest metal available. We recommend that you vent the moulds if you use Standard Metal. Standard metal melts at 210°C (410°F)... | 5 Star metal (94.5% Tin / 3% Zinc / 2.5% Antimony) is lead free. However it is more difficult to cast and we recommend that you vent all moulds. Melts at 230° C (446° F). Cast at... |